Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Applied Composites 8041 Polyester SMC

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Applied Composites Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Applied Composites 8041 Polyester SMC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Industry Application: ElectricalProduct Application: Business MachinesDistinct Features: UL 94-VO, Radiant Panel
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Linear Mold Shrinkage 0.00 cm/cm
0.00 in/in
Cold Part VS Cold Tool; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 50
50
ASTM D2583
Hardness, Rockwell M 110
110
ASTM D785
Tensile Strength, Ultimate 75.8 MPa
11000 psi
ASTM D638
Tensile Modulus 12.4 GPa
1800 ksi
ASTM D638
Flexural Strength 179 MPa
26000 psi
ASTM D790
Flexural Modulus 10.3 GPa
1500 ksi
Tangent; ASTM D790
Compressive Strength 172 MPa
25000 psi
ASTM D695
Izod Impact, Notched 7.47 J/cm
14.0 ft-lb/in
ASTM D256
Taber Abrasion, mg/1000 Cycles 0.60
0.60
% Loss 1000 Cycles; FTMS1091
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
400 °F
Flexural Load; ASTM D648
Flammability, UL94 V-0
V-0
1/4 in; UL746
V-0
V-0
1/8 in; UL746
V-0
V-0
1/16 in; UL746