Amco Amalloy B9575 is a clear performance copolymer with exceptional clarity and toughness.Very clear, high tensile and flexural strength.Information provided by Amco Plastic Materials.
Physical Properties Metric English Comments
Melt Flow 4.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
4.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength at Break 32.2 MPa
4670 psi
ASTM D638
Tensile Strength, Yield 43.9 MPa
6370 psi
ASTM D638
Elongation at Break 18 %
18 %
ASTM D638
Tensile Modulus 2.44 GPa
354 ksi
ASTM D638
Flexural Strength 67.0 MPa
9720 psi
ASTM D790
Flexural Modulus 2.24 GPa
325 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Optical Properties Metric English Comments
Haze 1.1 %

@Thickness 2.54 mm
1.1 %

@Thickness 0.100 in
ASTM D1003
Transmission, Visible 91.2 %

@Thickness 2.54 mm
91.2 %

@Thickness 0.100 in
ASTM D1003