Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 920 PC (Asia Pacific) Opaque colors, low viscosity, superior flame retardance. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 923A PC (Asia Pacific) Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Asia Pacific) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer (Asia Pacific) Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | ASTM D790 |
Polymer Resources PC-GP3-TFE5 Polycarbonate, 5% PTFE, High Flow, Wear Resistant Polycarbonate, General Purpose, High Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Asia Pacific) 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Europe-Africa-Middle East) 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX2571T PC Copolymer Transparent weatherable PC copolymer for blowmolding/extrusion. |
|||
Flexural Modulus | 2.24 - 2.55 GPa | 325 - 370 ksi | ASTM D790 |
Alcoa KAMA 4200 RPET
(discontinued **) CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Up to 100% recycled.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 920A PC (Asia Pacific) Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 943 PC (Asia Pacific) Opaque colors, medium viscosity, superior flame retardance. UV-stabilized. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | ASTM D790 |
PolyOne Lubri-Tech™ AT-000/5T Black Acetal-Copolymer, PTFE Lubricated
(discontinued **) Preliminary DataDescription/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | ASTM D790 |
PolyOne Lubri-Tech™ AT-000/5T-2S Acetal-Copolymer, PTFE/Silicone Lubricated
(discontinued **) Description/Features:PTFE/Silicone LubricatedInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | ASTM D790 |
Ravago Manufacturing Americas Hybrid B2026IU Polycarbonate + PBT Alloy Available in North America UV Stabilizer Good Impact Resistance RoHS Compliant Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | ASTM D790 |
PolyOne Lubri-Tech™ AT-000/20T Copolymer Acetal - 20% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML4539 PC Polycarbonate for aircraft applications requiring FAR 25.853a compliance. Injection moldable. Opaque colors. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX2531T PC Copolymer Transparent weatherable PC copolymer for blowmolding/extrusion. |
|||
Flexural Modulus | 2.24 - 13.8 GPa | 325 - 2000 ksi | Average value: 7.77 GPa Grade Count:36 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL SPN420 PPE+PS Superior Productivity plus heat and impact resistance. Excellent processability. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 365 PC+PET Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031"". |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® IQNH2900 PBT+PC Import Grade. UL94 V-0 Performance with Non-Brominated Flame Retardant. PCR% is up to 12% by using Valox iQ* resin. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Asia Pacific) Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | ASTM D790 |
Styron PULSEâ„¢ 2300 PT PC/ABS Engineering Resin Information provided by Styron |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX0844 PPE+PS (Asia Pacific) Automotive interiors. High heat/moisture resistant. consistant processability. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Europe-Africa-Middle East) Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DL0039EF PC LNP* Lubricomp* DL-0039EF is a compound based on Polycarbonate resin containing 15% PTFE. Characteristics of this grade include: Flame Retardant and Internally Lubricated. |