Advanced Polymer Alloys DURACRYN 8080 NC Thermoplastic Rubber

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer APA - Advanced Polymer Alloys
Trade Name DURACRYN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Advanced Polymer Alloys DURACRYN 8080 NC Thermoplastic Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Advanced Polymer Alloys
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
Instantaneous; ASTM D2240
Tensile Strength, Ultimate 17.2 MPa
2500 psi
ASTM D412
Elongation at Break 450 %
450 %
ASTM D412
100% Modulus 0.00552 GPa
0.800 ksi
ASTM D412
Graves Tear Strength 52.6 kN/m
300 pli
Die C; ASTM D624; DIN 53507
Compression Set 63 %
63 %
After 22 Hr at 23°C; ASTM D395
67 %

@Temperature 70.0 °C
67 %

@Temperature 158 °F
Method B, 22 hours; ASTM D395
Tensile Set 9.0 %
9.0 %
ASTM D412
Thermal Properties Metric English Comments
Clash Berg Stiffness Temperature -18.0 °C
-0.400 °F
At 10,000 psi; ASTM D1043