Thermal Properties Metric English Comments
Clash Berg Stiffness Temperature -18.0 °C
-0.400 °F
T-10000 Torsional stiffness ASTM D1043-72(1981)
DuPont Performance Polymers Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound  (d
Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato..
Clash Berg Stiffness Temperature -18.0 °C
-0.400 °F
T-10000 Torsional stiffness ASTM D1043-72(1981)
DuPont Performance Polymers Hypalon® 48 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound  (d
Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato..
Clash Berg Stiffness Temperature -18.0 °C
-0.400 °F
At 10,000 psi; ASTM D1043
Advanced Polymer Alloys DURACRYN 8080 NC Thermoplastic Rubber
Information provided by Advanced Polymer Alloys
Copyright © lookpolymers.com All Rights Reserved