Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 52.6 - 210 kN/m | 300 - 1200 pli | Average value: 124 kN/m Grade Count:18 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Graves Tear Strength | 52.6 kN/m @Temperature 23.9 °C |
300 pli @Temperature 75.0 °F |
Die C; ASTM D624 |
Advanced Polymer Alloys Alcryn® 4680 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Graves Tear Strength | 52.6 kN/m | 300 pli | Die C; ASTM D624; DIN 53507 |
Advanced Polymer Alloys DURACRYN 8080 NC Thermoplastic Rubber Information provided by Advanced Polymer Alloys |
|||
Graves Tear Strength | 52.6 kN/m | 300 pli | Die C; ASTM D624 |
Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane Features: Excellent blend partner for PVC and general adhesive and good physical properties.Uses: Flat die/cast film extrusion and hose jacketing, Calendaring/melt coating.Available in Americas, Eur.. |