Polymer Property : Graves Tear Strength = 52.6 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Graves Tear Strength 52.6 - 210 kN/m
300 - 1200 pli
Average value: 124 kN/m Grade Count:18
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Graves Tear Strength 52.6 kN/m

@Temperature 23.9 °C
300 pli

@Temperature 75.0 °F
Die C; ASTM D624
Advanced Polymer Alloys Alcryn® 4680 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Graves Tear Strength 52.6 kN/m
300 pli
Die C; ASTM D624; DIN 53507
Advanced Polymer Alloys DURACRYN 8080 NC Thermoplastic Rubber
Information provided by Advanced Polymer Alloys
Graves Tear Strength 52.6 kN/m
300 pli
Die C; ASTM D624
Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane
Features: Excellent blend partner for PVC and general adhesive and good physical properties.Uses: Flat die/cast film extrusion and hose jacketing, Calendaring/melt coating.Available in Americas, Eur..