Aclo Accutech Polypropylene Copolymer CP0436G40CL Glass Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0436G40CL Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
MD; ASTM D955
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Ash 40 %
40 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 91
91
ASTM D785
Tensile Strength at Break 57.0 MPa
8270 psi
ASTM D638
Tensile Strength, Yield 58.0 MPa
8410 psi
ASTM D638
Elongation at Break 9.0 %
9.0 %
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Tensile Modulus 4.000 GPa
580.1 ksi
ASTM D638
Flexural Strength 87.98 MPa
12760 psi
ASTM D790
Flexural Modulus 5.699 GPa
826.6 ksi
ASTM D790
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 158 °C
316 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 139 °C
282 °F