Material Notes:
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
MD; ASTM D955
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 124
124
ASTM D785
Tensile Strength at Break 68.0 MPa
9860 psi
ASTM D638
Tensile Strength, Yield 68.0 MPa
9860 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Tensile Modulus 2.899 GPa
420.5 ksi
ASTM D638
Flexural Strength 107.0 MPa
15520 psi
ASTM D790
Flexural Modulus 4.100 GPa
594.6 ksi
ASTM D790
Izod Impact, Notched 0.101 J/cm
0.190 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 91.1 °C
196 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 78.9 °C
174 °F
Users viewing this material also viewed the following: