Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 64.0 °C | 147 °F | Deflection temperature; load unknown. |
Abatron AboCast 50-16/AboCure 50-12 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/14 ratio. Pot life: 500 g, 38 min. at 25°C (77°F). Exothermic Peak 280°C (535°F). Hardens in 2-24 hours.. |