Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.84 GPa | 412 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87547 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87548 AS Polyvinyl Chloride, Rigid (PVC, Rigid) A transparent PVC profile compound, with reduced surface resistivity, resulting in unlikely attraction and adhesion of dust. Actual results on surface resistivity = 1.3x10^15.Information provided by.. |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87554 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | ASTM D790 |
Kleerdex Kydex® P55 Acrylic/PVC Extrusion Compound
(discontinued **) Weatherable profile extrusion compoundApplications: Extruded profiles requiring weatherability, high flexural modulus, and excellent flammability resistance. Features: Weatherability is dependent o.. |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | ASTM D790 |
LG Chemical LUCON PO-3000 Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Flexural Modulus | 2.84 GPa @Thickness 6.40 mm |
412 ksi @Thickness 0.252 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID GN1001AF PA6, Halogen Free Flame Retardant Feature: Injection Molding, PA6, Halogen Free Flame RetardantApplication: Electrical & Electronic (Switch)CAS No. 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN333HS Heat Resistant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Modulus | 2.84 GPa @Thickness 6.40 mm |
412 ksi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL HF5254A PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN173MC M/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN331F General Purpose Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Modulus | 2.84 GPa @Thickness 6.40 mm |
412 ksi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL HF3308C PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Che.. |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DZL24 PC LNP LUBRICOMP* DZL24 is a compound based on Polycarbonate resin containing 20% Milled Glass, 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA6.12 LNP* LUBRICOMP* IAL12 is a compound based on Nylon 6/12 resin containing 5% PTFE, 10% Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OL004 PPS - Linear LNP* LUBRICOMP* OL004 is a compound based on PPS - Linear resin containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RL002 PA 66 LNP LUBRICOMP* RL002 is a compound based on Nylon 66 resin containing 10% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON AX00756 ABS LNP STAT-KON* AX00756 is a compound based on ABS resin containing Stainless Steel. Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp FF004 PE LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® TF-0930 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | ASTM D790 |
Samyang Tribit® 1500G10 PBT, Reinforced General Purpose Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G10 is a reinforced, general purpose gr.. |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL LEN2211 PPE+HIPS (Asia Pacific) PPE / HIPS unfilled, FR for LED application |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP LNP THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 2.84 GPa @Thickness 3.20 mm |
412 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SC 202EL General Purpose Polystyrene CharacteristicsHigh strength grade Excellent process ability Reduces processing cycle timeProcessing MoldingApplicationsAudio cassettes housing and covers, CD jewel boxes Medical products like disp.. |
|||
Flexural Modulus | 2.84 GPa @Thickness 3.20 mm |
412 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SC 203 LV General Purpose Polystyrene CharacteristicsGood flow grade with good mechanical properties Good clarity and flexibility Easy processing grade and suitable for thin walled applicationsProcessing Extrusion MoldingApplicationsSu.. |
|||
Flexural Modulus | >= 2.84 GPa | >= 412 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 2121UV-M-31 Black Filled Polypropylene Homopolymer DescriptionPolyfort® FPP 2121UV-M-31 is a 30% black filled polypropylene homopolymer. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman... |
|||
Flexural Modulus | >= 2.84 GPa | >= 412 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 2121UV-M-31 Black Filled Polypropylene Homopolymer DescriptionPolyfort® FPP 2121UV-M-31 is a 30% black filled polypropylene homopolymer. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman... |
|||
Flexural Modulus | >= 2.84 GPa | >= 412 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 2121UV-M-31 Black Filled Polypropylene Homopolymer DescriptionPolyfort® FPP 2121UV-M-31 is a 30% black filled polypropylene homopolymer. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman... |
|||
Flexural Modulus | 2.84 GPa | 412 ksi | ASTM D790 |
Total PSC 1540(AS) Crystal Polystyrene 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact p.. |
|||
Flexural Modulus | >= 2.84 GPa | >= 412 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 2121UV-M-31 Black Filled Polypropylene Homopolymer DescriptionPolyfort® FPP 2121UV-M-31 is a 30% black filled polypropylene homopolymer. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman... |
|||
Flexural Modulus | 2.84 GPa @Temperature 23.0 °C |
412 ksi @Temperature 73.4 °F |
EN ISO 178 |
Ensinger TECASINT 3022 Polyimide, Black, 15% Graphite (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Flexural Modulus | 2.84 GPa @Thickness 3.20 mm |
412 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 6630 Antistatic Polystyrene Characteristics Easy flow Excellent transparency Processing Extrusion Applications For glossy cap layer on HIPS To prevent dust patterns on thermoformed products Material Status: Commercial : Acti.. |