Aaron Industries AVPS H 100-3 Virgin Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer Aaron Industries Corporation
Trade Name AVPS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AVPS H 100-3 Virgin Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melt flow index may be specified.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 4.0 - 12 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.0 - 12 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 42.7 MPa
6200 psi
ASTM D638
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Izod Impact, Notched 0.854 - 1.60 J/cm
1.60 - 3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C
226 °F
ASTM D648
Users viewing this material also viewed the following: