Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aaron Industries AAROPRENE® CFPP 2020 Calcium Carbonate Filled Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Manufacturer Aaron Industries Corporation
Trade Name AAROPRENE® CFPP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROPRENE® CFPP 2020 Calcium Carbonate Filled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AAROPRENE® CFPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Filler Content 20 %
20 %
Calcium Carbonate; ASTM D2584
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Melt Flow 8.0 - 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 - 12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 29.0 MPa
4200 psi
ASTM D638
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched 0.411 J/cm
0.770 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C
210 °F
ASTM D648