AK Steel ZINCGRIP® FORMABLE 50K / ASTM A1008 class 1 / SAE J1392 050 XLK, Grade 50 Electrogalvanized Carbon Steel, High Strength Low Alloy Steel (HSLAS)

Category Metal , Ferrous Metal , Carbon Steel , Low Carbon Steel
Manufacturer AK Steel
Trade Name ZINCGRIP®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AK Steel ZINCGRIP® FORMABLE 50K / ASTM A1008 class 1 / SAE J1392 050 XLK, Grade 50 Electrogalvanized Carbon Steel, High Strength Low Alloy Steel (HSLAS).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 450 MPa
>= 65300 psi
Tensile Strength, Yield >= 345 MPa
>= 50000 psi
Elongation at Break >= 20 %
>= 20 %
Modulus of Elasticity 200 GPa
29000 ksi
Thermal Properties Metric English Comments
CTE, linear 12.4 µm/m-°C

@Temperature 20.0 - 100 °C
6.89 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.481 J/g-°C

@Temperature 50.0 - 100 °C
0.115 BTU/lb-°F

@Temperature 122 - 212 °F
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000142 ohm-cm
0.0000142 ohm-cm
Users viewing this material also viewed the following: