Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.4 µm/m-°C @Temperature 25.0 - 700 °C |
6.89 µin/in-°F @Temperature 77.0 - 1290 °F |
|
Du-Co Ceramics S-464 Magnesia Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 1011, Grade 50 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 1011, Grade 55 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 1018, Grade 30 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 1018, Grade 36 Type 1 and 2 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 607 Class 1 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 607 Class 1 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 607 Class 1 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 607 Class 2 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 607 Class 2 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 607 Class 2 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 715 Class 2 Formable, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 715 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel CL 1/ SAE J1392 045 XLK, Grade 45 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel SAE J1392 040XLK or 040YLK, Grade 40 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel SAE J1392, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) AK Steel Formable Grade - F indicates inclusion controlled low alloy.Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ZINCGRIP® FORMABLE 50K / ASTM A1008 class 2 / SAE J1392 050 XLK, Grade 50 Electrogalvanized Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, High Strength Low Alloy Steel (HSLA), 040XLK SAE Specified properties not covered by ASTMInformation provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, High Strength Low Alloy Steel (HSLA), 045XLK SAE Specified properties not covered by ASTMInformation provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 1011, Class 1 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 1011, Class 1 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 1011, Class 1 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 1011, Class 1 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 1011, Grade 33 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 1011, Grade 40 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 1018, Grade 40 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel CL 2/ SAE J1392 045 XLK, Grade 45 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |