Polymer Property : Rupture Strength = 23.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Rupture Strength 23.0 MPa

@Temperature 900 °C,
Time 3.60e+7 sec
3340 psi

@Temperature 1650 °F,
Time 10000 hour
Stress Rupture
AFE Technologies Cronite 657 Nickel Alloy Castings
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..
Rupture Strength 23.0 MPa

@Temperature 900 °C,
Time 3.60e+7 sec
3340 psi

@Temperature 1650 °F,
Time 10000 hour
Stress Rupture
AFE Technologies Cronite 37Ni/18Cr No. HR5
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..