Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 23.0 MPa @Temperature 900 °C, Time 3.60e+7 sec |
3340 psi @Temperature 1650 °F, Time 10000 hour |
Stress Rupture |
AFE Technologies Cronite 657 Nickel Alloy Castings High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF.. |
|||
Rupture Strength | 23.0 MPa @Temperature 900 °C, Time 3.60e+7 sec |
3340 psi @Temperature 1650 °F, Time 10000 hour |
Stress Rupture |
AFE Technologies Cronite 37Ni/18Cr No. HR5 High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF.. |