Mechanical Properties Metric English Comments
Rupture Strength 64.0 MPa

@Temperature 750 °C,
Time 3.60e+7 sec
9280 psi

@Temperature 1380 °F,
Time 10000 hour
Stress Rupture
AFE Technologies Cronite 657 Nickel Alloy Castings
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..