Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ACC SMP™ EP 3001 EPI Engineered Polymers Silicone Modified Polymer

Category Polymer , Thermoset , Silicone
Manufacturer Amber Chemical Company
Trade Name SMP™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC SMP™ EP 3001 EPI Engineered Polymers Silicone Modified Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EP 3001, “Powered by Reactamine® Technology”, is a two component 100% solid polyurea based sealant. EP 3001 is a self-leveling sealant designed to protect horizontal concrete. This elastomer displays fast cure times and excellent adhesion to concrete. EP-3001 can be applied at temperatures ranging 30° F to 120°F. This elastomer displays excellent chemical resistance and water insensitivity. EP-3001 may also be used under traditional floor coatings (such as epoxies, polyureas and polyurethanes) or tiles to provide protection from cracking and sinking caused by non-elastomeric sealants. Applications: EP 3001 was designed to protect against the abuse to concrete caused by heavy load transfers from such items as forklifts, steel-wheeled carts and trash dumpsters. Some typical uses include: Concrete Water Proofing Concrete Spall Repairs Cold Storage Facilities Merchandise Distribution Centers Home Improvement Stores Bridge Headers Warehouse Floors U.S.D.A. and F.D.A. AcceptablePart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Viscosity 1200 cP
1200 cP
B Side
1800 cP
1800 cP
A Side
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D2240
Tensile Strength, Yield 10.3 MPa
1500 psi
ASTM D412
Elongation at Break 800 %
800 %
ASTM D412
100% Modulus 0.00965 GPa
1.40 ksi
ASTM D412
Adhesive Bond Strength >= 2.76 MPa
>= 400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
Tear Strength 78.9 kN/m
450 pli
ASTM D412
Taber Abrasion, mg/1000 Cycles 20.5
20.5
CS17 WHEEL, 1kg per 1000 cycles; ASTM D4060
Thermal Properties Metric English Comments
Flash Point >= 93.3 °C
>= 200 °F
ASTM Pensky-Martin
Processing Properties Metric English Comments
Cure Time >= 10.0 min
>= 0.167 hour
Tack Free Time
Gel Time 5.00 min
5.00 min
Descriptive Properties Value Comments
Color Black, Charcoal Gray, Light Gray
Flexibility Pass
ASTM D1737, 1/8"Mandrel
Resistance to Acetic Acid (100%) Recommended
Resistance to Brake Fluid (310g/l) Recommended Conditional
Resistance to Clorox® (10%) H2O Conditional, Discoloration
Resistance to Diesel Fuel Recommended
Resistance to Gasoline Recommended
Resistance to H2O Recommended
Resistance to Hydraulic Fluid (oil) Recommended, Discoloration
Resistance to Hydrochloric Acid (10%) Recommended
Resistance to Mineral Spirits Recommended
Resistance to Motor Oil Recommended, Discoloration
Resistance to Muriatic Acid (10%) Recommended
Resistance to NaCl/H2O (10%) Recommended
Resistance to Potassium Hydroxide (10%) Recommended
Resistance to Sodium Bicarbonate Recommended
Resistance to Sodium Hydroxide (10%) Recommended
Resistance to Sugar/H2O Recommended
Resistance to Sulfuric Acid (>22%) Not Recommended
Resistance to Sulfuric Acid (10%) Recommended, Discoloration
Resistance to Vinegar/ H2O (5%) Recommended
Resistance to Xylene Conditional