Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.223 g/cc | 1.223 g/cc | ASTM D792 |
Noble Polymers Ecobarrier™ 0512 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Specific Gravity | 1.223 g/cc | 1.223 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene DescriptionPolyfort® FPP 3443U is a 40% talc fortified UV resistant homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Specific Gravity | 1.223 g/cc | 1.223 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene DescriptionPolyfort® FPP 3443U is a 40% talc fortified UV resistant homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Specific Gravity | 1.223 g/cc | 1.223 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene DescriptionPolyfort® FPP 3443U is a 40% talc fortified UV resistant homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Specific Gravity | 1.223 g/cc | 1.223 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene DescriptionPolyfort® FPP 3443U is a 40% talc fortified UV resistant homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Specific Gravity | 1.223 g/cc | 1.223 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene DescriptionPolyfort® FPP 3443U is a 40% talc fortified UV resistant homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Specific Gravity | 1.223 g/cc | 1.223 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene DescriptionPolyfort® FPP 3443U is a 40% talc fortified UV resistant homopolymer polypropylene product. Information provided by A. Schulman. |