Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® NN100HSL (COND, 50% RH) Nylon 66, Heat Stabilized, Internally Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® NN100HSL (COND, 50% RH) Nylon 66, Heat Stabilized, Internally Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chase Plastics.
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.5 MPa
9500 psi
ASTM D638
Elongation at Break >= 150 %
>= 150 %
ASTM D638
Flexural Strength 42.1 MPa
6100 psi
ASTM D790
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 232 °C
450 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C
180 °F
ASTM D648