Material Notes:
Description: UBESTA Nylon 12 CopolymerInformation provided by UBE.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Melt Flow 4.2 g/10 min

@Load 1.00 kg,
Temperature 190 °C
4.2 g/10 min

@Load 2.20 lb,
Temperature 374 °F
ASTM D1238R
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 27.0 MPa
>= 3920 psi
ASTM D638
Tensile Strength, Yield 9.00 MPa
1310 psi
ASTM D638
Elongation at Break >= 300 %
>= 300 %
ASTM D638
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
Flexural Modulus 0.780 GPa
113 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 135 °C
275 °F
ASTM D3418