A. Schulman POLYBATCH™ White P8555 T2 Concentrate Based In Homopolymer Polypropylene

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ White P8555 T2 Concentrate Based In Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBATCH® P8555 T2 is a premium white masterbatch containing 50% TiO2 based in homopolymer polypropylene. This product is processed through 300x300 mesh screens and offers premium dispersion POLYBATCH® P8555 T2 is recommended for use in cast, blown, OPP, or BOPP film applications requiring high loading levels with premium dispersion. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 50 %
50 %
Descriptive Properties Value Comments
Moisture (max) 500
ppm, ASTM D789
Pellet Count 36
pellets/gram