A. Schulman POLYBATCH™ Deep Red 50389 Concentrate Based In Linear Low-Density Polyethylene

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ Deep Red 50389 Concentrate Based In Linear Low-Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DescriptionPOLYBATCH® 50389 is a deep red color concentrate based in linear low density polyethylene. This product was formulated to offer color in polyethylene film applications. POLYBATCH® 50389 is typically recommended for use at 28% addition levels. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 7.0 %
7.0 %
Descriptive Properties Value Comments
Moisture (max) 1000
ppm, ASTM D789
Pellet Count 55
pellets/gram