Mechanical Properties Metric English Comments
Flexural Modulus 0.0593 GPa
8.60 ksi
at 1% secant modulus; ASTM D790
A. Schulman POLYAXIS® LPA815 LPA 815EVA
DescriptionPolyaxis LPA 815 is an EVA which is soft an pliable, even at low temperatures.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR ..
Flexural Modulus 0.0593 GPa
8.60 ksi
at 1% secant modulus; ASTM D790
A. Schulman POLYAXIS® LPA815 LPA 815EVA
DescriptionPolyaxis LPA 815 is an EVA which is soft an pliable, even at low temperatures.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR ..
Flexural Modulus 0.0593 GPa
8.60 ksi
at 1% secant modulus; ASTM D790
A. Schulman POLYAXIS® LPA815 LPA 815EVA
DescriptionPolyaxis LPA 815 is an EVA which is soft an pliable, even at low temperatures.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR ..
Flexural Modulus 0.0593 GPa
8.60 ksi
at 1% secant modulus; ASTM D790
A. Schulman POLYAXIS® LPA815 LPA 815EVA
DescriptionPolyaxis LPA 815 is an EVA which is soft an pliable, even at low temperatures.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR ..
Flexural Modulus 0.0593 GPa
8.60 ksi
ASTM D790
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUses: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Flexural Modulus 0.0593 GPa
8.60 ksi
at 1% secant modulus; ASTM D790
A. Schulman POLYAXIS® LPA815 LPA 815EVA
DescriptionPolyaxis LPA 815 is an EVA which is soft an pliable, even at low temperatures.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR ..
Flexural Modulus 0.0593 GPa
8.60 ksi
at 1% secant modulus; ASTM D790