A. Schulman ComAlloy Hiloy® 275 Polystyrene Alloy, Mineral Reinforced, Flow Enhanced

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Glass Filled
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Hiloy® 275 Polystyrene Alloy, Mineral Reinforced, Flow Enhanced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.30% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Ultimate 63.0 MPa
9140 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Flexural Strength 101 MPa
14600 psi
ASTM D790
Flexural Modulus 7.10 GPa
1030 ksi
ASTM D790
Izod Impact, Unnotched 1.39 J/cm
2.60 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 103 °C
217 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 216 - 241 °C
421 - 466 °F