3M Scotchkote™ 413/215 Patch Compound

Category Other Engineering Material
Manufacturer 3M
Trade Name Scotchkote™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ 413/215 Patch Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by 3M
Physical Properties Metric English Comments
Solids Content 56.2 %
56.2 %
Volatile Organic Compounds (VOC) Content 271 g/l
271 g/l
Viscosity 1400 - 1550 cP
1400 - 1550 cP
Mixed
Thermal Properties Metric English Comments
Flash Point 36.0 °C
96.8 °F
Closed Cup, Part A
60.0 °C
140 °F
Closed Cup, Part B
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Light Green