Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1050 - 1550 cP | 1050 - 1550 cP | 25% Toluene Solution at 25°C; BAM 922 |
Kraton® G1642 H (SEBS) Linear Triblock Copolymer Description: Kraton G1642 H is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 20%. It is supplied from North America in the physical form ide.. |
|||
Viscosity | 1250 - 1550 cP @Temperature 60.0 °C |
1250 - 1550 cP @Temperature 140 °F |
|
C.O.I.M. DIEXTER® G214 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 1400 - 1550 cP | 1400 - 1550 cP | Mixed |
3M Scotchkote™ 413/215 Patch Compound Information provided by 3M |