Polymer Property : Volatile Organic Compounds (VOC) Content = 271 g/l
Polymer Property :
Volatile Organic Compounds (VOC) Content =
271 g/l
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Volatile Organic Compounds (VOC) Content
271
g/l
271
g/l
3M Scotchkote™ 413/215 Patch Compound
Information provided by 3M