Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 159 min @Temperature 24.0 °C |
2.65 hour @Temperature 75.2 °F |
Dry to Handle Time; ASTM D1640 clause 7.7.1 |
3M Scotchkote™ 323 Purple Patch Compound 3M Scotchkote 323 Purple Patch Compound is an ambient temperature cure, two-part system designed to protect metal, concrete and other surfaces from corrosion and deterioration. Scotchkote 323 Purple.. |