3M Scotch-Weld™ 1838 B/A Green Two-Part Structural Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ 1838 B/A Green Two-Part Structural Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-purpose and Rigid bondsInformation provided by 3M
Physical Properties Metric English Comments
Viscosity 400000 cP
400000 cP
Mechanical Properties Metric English Comments
Shear Strength 3.45 MPa

@Temperature 82.0 °C
500 psi

@Temperature 180 °F
Overlap
10.3 MPa

@Temperature -55.0 °C
1500 psi

@Temperature -67.0 °F
Overlap
20.7 MPa

@Temperature 24.0 °C
3000 psi

@Temperature 75.2 °F
Overlap
Peel Strength 0.701 kN/m
4.00 pli
T-Peel
Processing Properties Metric English Comments
Cure Time 480 min
8.00 hour