Mechanical Properties Metric English Comments
Shear Strength 3.45 MPa

@Temperature 100 °C
500 psi

@Temperature 212 °F
Tensile lap
Resin Technology Group TIGA 110-EXDP Low Viscosity, Optically Clear Glass Bonder
Mix ratio 100/50 by volume.TIGA 110EX-DP is a transparent, low viscosity epoxy resin formulation recommended for industrial adhesive, small potting and laminating applications where sparkling clarit..
Shear Strength >= 3.45 MPa

@Temperature 93.3 °C
>= 500 psi

@Temperature 200 °F
Tensile, Al to Al
Master Bond EP3HTS Silver Filled, Electrically Conductive Epoxy
Description: Master Bond Polymer System EP3HTS is a one component, silver filled, electrically conductive epoxy system featuring high shear strength and good temperature resistance along with a fast..
Shear Strength 3.45 MPa

@Temperature 82.0 °C
500 psi

@Temperature 180 °F
Overlap
3M Scotch-Weld™ 1838 B/A Green Two-Part Structural Adhesive
Multi-purpose and Rigid bondsInformation provided by 3M
Shear Strength 3.45 MPa

@Temperature 82.0 °C
500 psi

@Temperature 180 °F
Overlap
3M Scotch-Weld™ 1838 B/A Tan Two-Part Structural Adhesive
Multi-purpose and Rigid bondsInformation provided by 3M
Shear Strength >= 3.45 MPa

@Temperature 93.3 °C
>= 500 psi

@Temperature 200 °F
Tensile, Al to Al
Master Bond EP3HTSMed Silver Filled, Medical Grade Epoxy
Description: Master Bond EP3HTSMed is a one component, silver filled, electrically conductive epoxy system featuring high shear strength and good temperature resistance along with a fast cure schedu..