3M SJ6100 Protective Product, Molded Shapes

Category Other Engineering Material
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M SJ6100 Protective Product, Molded Shapes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many applications. The urethane is a durable, resilient elastomer. The aggressive, high tack, pressure sensitive adhesive is protected with a release liner making application fast and easy.Information provided by 3M
Mechanical Properties Metric English Comments
Hardness, Shore M 72
72
ASTM D2240
Tensile Strength at Break 4.10 MPa
595 psi
Die A; ASTM D412
Elongation at Break 100 %
100 %
Die A; ASTM D412
Coefficient of Friction >= 1.0
>= 1.0
Stainless Steel, Kinetic; ASTM D1894
>= 1.0
>= 1.0
Glass, Kinetic; ASTM D1894
0.90 - 1.4
0.90 - 1.4
Formica laminate, Kinetic; ASTM D1894
0.90 - 1.4
0.90 - 1.4
Wood, Kinetic; ASTM D1894
Peel Strength 9.12 kN/m
52.0 pli
90°, Adhesion to Polypropylene
9.64 kN/m
55.0 pli
90°, Adhesion to Polystyrene
9.64 kN/m
55.0 pli
90°, Adhesion to ABS
9.64 kN/m
55.0 pli
90°, Adhesion to Stainless Steel
9.64 kN/m
55.0 pli
90°, Adhesion to Aluminum
Taber Abrasion, mg/1000 Cycles 1.7 - 1.9
1.7 - 1.9
H18, 1 kg; ASTM C501
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 52.0 °C
126 °F
Application
66.0 °C
151 °F
Service
107 °C
225 °F
Intermittent
Minimum Service Temperature, Air -34.0 °C
-29.2 °F
Service
5.00 °C
41.0 °F
Application
Electrical Properties Metric English Comments
Dielectric Strength 7.87 kV/mm
200 kV/in
ASTM D1000