Mechanical Properties Metric English Comments
Peel Strength 9.12 kN/m

@Temperature 21.1 °C
52.0 pli

@Temperature 70.0 °F
Bell Peel
Hexcel® Redux® 312 Modified epoxy film adhesive (0.06 psf)
Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support..
Peel Strength 9.12 kN/m

@Temperature 21.1 °C
52.0 pli

@Temperature 70.0 °F
Bell Peel
Hexcel® Redux® 312UL Modified epoxy film adhesive
Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support..
Peel Strength 9.12 kN/m

@Temperature 21.1 °C
52.0 pli

@Temperature 70.0 °F
Hexcel® Redux® 335K Adhesive film for bonding metallic and composite components (0.03 psf)
Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a..
Peel Strength 9.12 kN/m

@Temperature 21.1 °C
52.0 pli

@Temperature 70.0 °F
Hexcel® Redux® 335U Adhesive film for bonding metallic and composite components (0.03 psf)
Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a..
Peel Strength 9.12 kN/m
52.0 pli
90°, Adhesion to Polypropylene
3M Bumpon™ SJ5208 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 9.12 kN/m
52.0 pli
90°, Adhesion to Polypropylene
3M Bumpon™ SJ5216 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 9.12 kN/m
52.0 pli
90°, Adhesion to Polypropylene
3M Bumpon™ SJ6216 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 9.12 kN/m
52.0 pli
180°, Aluminum
3M Scotch-Weld™ TE040 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Peel Strength 9.12 kN/m
52.0 pli
90°, Adhesion to Polypropylene
3M SJ5201 Protective Product, Die Cut Shapes
3M Bumpon Protective Products SJ5201 and SJ5202 are pressure-sensitive, adhesive backed polyurethane products made from SJ5200 Series soft foam rollstock. A hexagon shape is often preferred for vari..
Peel Strength 9.12 kN/m
52.0 pli
90°, Adhesion to Polypropylene
3M SJ6100 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Peel Strength 9.12 kN/m
52.0 pli
90°, Adhesion to Polypropylene
3M SJ6344 Protective Product, Molded Shapes
3M Bumpon Protective Products SJ6344 is a pressure-sensitive adhesive-backed, molded polyurethane product. The Bumpon SJ6344 is called an Easy Slide Series because it incorporates a special abrasion..
Peel Strength 9.12 kN/m
52.0 pli
90°, Adhesion to Polypropylene
3M Bumpon™ SJ6208 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 9.12 kN/m
52.0 pli
90°, Adhesion to Polypropylene
3M Bumpon™ SJ6232 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Peel Strength 9.12 kN/m
52.0 pli
90°, Adhesion to Polypropylene
3M SJ5202 Protective Product, Die Cut Shapes
3M Bumpon Protective Products SJ5201 and SJ5202 are pressure-sensitive, adhesive backed polyurethane products made from SJ5200 Series soft foam rollstock. A hexagon shape is often preferred for vari..