Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 4.10 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 4.10 MPa
595 psi
Certified
NuSil MED-6033 Silicone, Low Consistency Elastomer - Restricted Medical Use
Description: Low consistency elastomers (LCEs) are useful alternatives to liquid silicone rubber (LSR) and high consistency rubber (HCR) for end users who need a low viscosity elastomer which provid..
Tensile Strength at Break 4.10 MPa
595 psi
Certified
NuSil MED-6233 Low Consistency Elastomer - Unrestricted Medical Use
Description: Low consistency elastomers (LCEs) are useful alternatives to liquid silicone rubber (LSR) and high consistency rubber (HCR) for end users who need a low viscosity elastomer which provid..
Tensile Strength at Break 4.10 MPa
595 psi
Certified
NuSil MED-6607 Dispersion - Unrestricted Medical Use
Description: “Dispersion” is a term used to describe a silicone elastomer system that is suspended or dispersed in a solvent carrier. It is a complex solution that contains silicone polymers of va..
Tensile Strength at Break 4.10 MPa
595 psi
Certified
NuSil MED-6655 Dispersion - Unrestricted Medical Use
Description: “Dispersion” is a term used to describe a silicone elastomer system that is suspended or dispersed in a solvent carrier. It is a complex solution that contains silicone polymers of va..
Tensile Strength at Break 4.10 MPa

@Temperature 23.0 °C
595 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 1060X-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 1060X-1 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, ABS, PC/ABSColor conce..
Tensile Strength at Break 4.10 MPa
595 psi
NuSil CF2-3521-2 Fluorosilicone
General Purpose: Thermally ConductiveComments: Fuel ResistantCure System: PlatinumInformation provided by NuSil
Tensile Strength at Break 4.10 MPa
595 psi
NuSil CV-2510 Silicone, Two Part Adhesive and Sealant
General Purpose: Two Part Adhesive and SealantComments: Low/High Temperature, FlowableCure system: AlkoxyInformation provided by NuSil
Tensile Strength at Break 4.10 MPa
595 psi
NuSil EPM-2422 Silicone, Potting & Encapsulating Material
General Purpose: Potting & Encapulating MaterialsCure system: PlatinumInformation provided by NuSil
Tensile Strength at Break 4.10 MPa
595 psi
NuSil Lightspan™ LS-6143 Silicone, Optical Adhesive Elastomer
General Purpose: Optical Adhesives and ElastomerComments: Broad opearting temperature rangeApplications: Bonding, EncapsulantInformation provided by NuSil
Tensile Strength at Break 4.10 MPa
595 psi
Certified
NuSil MED-1055 Silicone, One Part Adhesive/Sealant - Restricted Medical Use
Silicone adhesives are elastomers or pressure sensitive adhesive systems that are designed to bond silicone surfaces to each other and to other substrate surfaces such as metals and plastics. There ..
Tensile Strength at Break 4.10 MPa
595 psi
Certified
NuSil MED10-6607 Dispersion - Restricted Medical Use
Description: “Dispersion” is a term used to describe a silicone elastomer system that is suspended or dispersed in a solvent carrier. It is a complex solution that contains silicone polymers of va..
Tensile Strength at Break 4.10 MPa
595 psi
Certified
NuSil MED10-6655 Dispersion - Restricted Medical Use
Description: “Dispersion” is a term used to describe a silicone elastomer system that is suspended or dispersed in a solvent carrier. It is a complex solution that contains silicone polymers of va..
Tensile Strength at Break 4.10 MPa
595 psi
Certified
NuSil MED-1555 Silicone, One part Adhesive - Unrestricted Medical Use
Description: Silicone adhesives are elastomers or pressure sensitive adhesive systems that are designed to bond silicone surfaces to each other and to other substrate surfaces such as metals and pla..
Tensile Strength at Break 4.10 MPa
595 psi
Certified
NuSil MED-4044 Silicone, Low Consistency Elastomer - Restricted Medical Use
Description: Low consistency elastomers (LCEs) are useful alternatives to liquid silicone rubber (LSR) and high consistency rubber (HCR) for end users who need a low viscosity elastomer which provid..
Tensile Strength at Break 4.10 MPa
595 psi
Certified
NuSil MED-4244 Low Consistency Elastomer - Unrestricted Medical Use
Description: Low consistency elastomers (LCEs) are useful alternatives to liquid silicone rubber (LSR) and high consistency rubber (HCR) for end users who need a low viscosity elastomer which provid..
Tensile Strength at Break 4.10 MPa
594 psi
Air at 212°F, 168 hr; ASTM D573
ExxonMobil Santoprene® 281-45MED Thermoplastic Elastomer  (discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad..
Tensile Strength at Break 4.10 MPa

@Time 7200 sec
594 psi

@Time 2.00 hour
Die C; ASTM D414
STAR Thermoplastic Alloys & Rubbers StarCLEAR CLR-1050 TPE
Product Description: StarCLEAR CLR-1050 is an easy processing TPE designed for injection molding. Soft and ultra clear TPEs specifically targeted to medical, consumer and sporting goods market. Feat..
Tensile Strength at Break 4.10 MPa
595 psi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 3460 Thermoplastic Elastomer
A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject..
Tensile Strength at Break 4.10 MPa
595 psi
ISO 37
ELASTO UK Dryflex® 3037-111 TPE, Modified Injection Molding Grade for Auto Interior Parts
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3037-111 is specifically designe..
Tensile Strength at Break 4.10 MPa
595 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8191-55B100 Thermoplastic Elastomer
A soft, black, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/PS b..
Tensile Strength at Break 4.10 MPa
595 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8211-55B100 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/..
Tensile Strength at Break 4.10 MPa
595 psi
ASTM D412
Diamond Polymers Softflex® 6001 Thermoplastic Elastomer Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength at Break 4.10 MPa
595 psi
Die A; ASTM D412
3M SJ5500 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Tensile Strength at Break 4.10 MPa
595 psi
Die A; ASTM D412
3M SJ5700 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Tensile Strength at Break 4.10 MPa
595 psi
Die A; ASTM D412
3M SJ6100 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Tensile Strength at Break 4.10 MPa
595 psi
Die A; ASTM D412
3M SJ5000 Protective Product, Molded Shapes
3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a..
Tensile Strength at Break 4.10 MPa

@Time 7200 sec
594 psi

@Time 2.00 hour
Die C; ASTM D414
STAR Thermoplastic Alloys & Rubbers StarCLEAR CLR-1040 TPE
Product Description: StarCLEAR CLR-1040 is an easy processing TPE designed for injection molding. Soft and ultra clear TPEs specifically targeted to medical, consumer and sporting goods market. Feat..
Copyright © lookpolymers.com All Rights Reserved