Material Notes:
Dyneon™ TF 2073 Z PTFE is an ideal grade for the manufacture of high quality micro tubing as well as wire and cable insulations. This product is also ideal for very thin-wall, smallest diameter tubing with maximum reduction ratio of up to 4200:1.Product Features: Needs less lubricant than TF 2072 Z PTFE Emulsion polymerization PTFE Product grade with lower extrusion pressure than TF 2070 Z PTFE Wide processing range Processing by standard paste extrusion methods Meets ASTM D4895-04 Type 1, Grade 1, Class C classification High molecular weightInformation provided by 3M
Physical Properties Metric English Comments
Bulk Density 0.490 g/cc
0.0177 lb/in³
DIN EN ISO 60
Density 2.17 g/cc
0.0784 lb/in³
DIN EN ISO 12086
Particle Size 430 µm
430 µm
ISO 13320
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa
5080 psi
DIN EN ISO 527-3
Elongation at Break 460 %
460 %
DIN EN ISO 527-3
Descriptive Properties Value Comments
Extrusion pressure @ RR 400:1 30 MPa
@ RR 400:1
Range of Reduction Ratios (RR) 50-4200:1