Polymer Property : Bulk Density = 0.0177 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.490 g/cc
0.0177 lb/in³
Zircar Zirconia ALK-15 Alumina Knit Textile Insulation
Alumina (Al2 O3) has excellent thermal shock resistance, high dimensional stability and good chemical inertness, which makes our alumina fiber products ideal for fast firing cycles up to 1700°C. Ou..
Bulk Density 0.490 g/cc
0.0177 lb/in³
DIN-53466
Iran Petrochemical (PCC) PVC-S7054 Poly Vinyl Chloride
Grade S-7054 has high porosity. Therefore it is most suitable for flexible applications. The electrical, mechanical & thermal properties expected of the various applications can be achieved with th..
Bulk Density 0.490 g/cc
0.0177 lb/in³
Zircar Zirconia ALK-15 Alumina Knit Textile Insulation
Alumina (Al2 O3) has excellent thermal shock resistance, high dimensional stability and good chemical inertness, which makes our alumina fiber products ideal for fast firing cycles up to 1700°C. Ou..
Bulk Density 0.490 g/cc
0.0177 lb/in³
DIN EN ISO 60
3M Dyneon™ TF 2073Z PTFE Fine Powder
Dyneon™ TF 2073 Z PTFE is an ideal grade for the manufacture of high quality micro tubing as well as wire and cable insulations. This product is also ideal for very thin-wall, smallest diameter tub..
Bulk Density 0.490 g/cc
0.0177 lb/in³
Asahi Glass Fluon® RB2510 10% Carbon Fiber, PTFE Filled Compound
Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc.