Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00710 GPa | 1.03 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 3190 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3190 can be processed by blow molding, injection molding or.. |
|||
100% Modulus | 0.00710 GPa | 1.03 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 3490N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
100% Modulus | 0.00710 GPa | 1.03 ksi | ISO 37 |
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00710 GPa | 1.03 ksi | |
Colorite Polymers Self Frosting™ 7511SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
100% Modulus | 0.00710 GPa | 1.03 ksi | |
Colorite Polymers 7511 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
100% Modulus | 0.00710 GPa | 1.03 ksi | |
Colorite Polymers 7512 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
100% Modulus | 0.00710 GPa | 1.03 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FE 5623 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5623 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
100% Modulus | 0.00710 GPa | 1.03 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FG 5690Q Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FG 5690Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |
|||
100% Modulus | 0.00710 GPa | 1.03 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 3490 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
100% Modulus | 0.00710 GPa | 1.03 ksi | Cured 7 min at 177°C and Post Cured 16 hr at 232°C |
DuPont Performance Polymers VTR 8525 (GBLT-S) GFLT-600 Formulation
(discontinued **) FormulationViton® GFLT 600 |