Material Notes:
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugations and rivets – Stretch selected finished graphic constructions up to 130% (ie a 10in film piece can stretch to 13 inches) without primer or relief cuts and maintain lift resistance; see details and exceptions in Section 8; Films IJ180C-10 and IJ180Cv3-10 have Comply™ Adhesive air release channels for fast, easy, bubble-free installations; Removable with heat and/or chemicalsInformation provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
without adhesive
76.2 - 102 microns
3.00 - 4.00 mil
with adhesive
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.2 MPa
2490 psi
Peel Strength 0.526 - 0.701 kN/m
3.00 - 4.00 pli
Adhesion to Acrylic enamel
0.526 - 0.877 kN/m
3.00 - 5.00 pli
Adhesion to Fruehauf pre-painted panels
0.701 - 0.877 kN/m
4.00 - 5.00 pli
Adhesion to ABS
0.701 - 0.877 kN/m
4.00 - 5.00 pli
Adhesion to Chrome
0.877 - 1.05 kN/m
5.00 - 6.00 pli
Adhesion to Aluminum, etched
1.23 - 1.40 kN/m
7.00 - 8.00 pli
Adhesion to Aluminum, anodized
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 32.0 °C
89.6 °F
Compound curves and/or watercraft
38.0 °C
100 °F
Flat without rivets
38.0 °C
100 °F
Curves or corrugations with rivets
Minimum Service Temperature, Air 4.00 °C
39.2 °F
Flat without rivets
10.0 °C
50.0 °F
Curves or corrugations with rivets
16.0 °C
60.8 °F
Compound curves and/or watercraft
Users viewing this material also viewed the following: