Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ 180Cv2-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ FN180C-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, etched |
3M Scotchcal™ IJ780Cv3 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-sensitive adhesive with non-visible, air release channels for fast, easy, bubble-free installations; Confirms to flat s.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ 180C Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ FN180Cv3-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ IJ180-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ IJ180C-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ IJ180Cv3-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ IJ380Cv3 Wrap Film with Comply™ v3 Adhesive 2-mil white, vinyl film with a luster finish; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Non-visible, air release channels for fast, easy, bubble-free installa.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ RG180-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ RG180C-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 1.23 - 1.40 kN/m | 7.00 - 8.00 pli | Adhesion to Aluminum, anodized |
3M Controltac™ 180 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |