Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 9673 Adhesive Transfer Tapes with Adhesive 300

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 9673 Adhesive Transfer Tapes with Adhesive 300.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive family is available in several thicknesses for a wide variety of surface bonding and provides a variety of liner confiations to help ensure excellent process flexibility.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Adhesive
152 microns
6.00 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.351 kN/m
2.00 pli
Polypropylene, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330
0.394 kN/m
2.25 pli
Polypropylene, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330
0.55877 kN/m
3.1875 pli
Stainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330
0.55877 kN/m
3.1875 pli
Polycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330
0.82172 kN/m
4.6875 pli
Polycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330
0.93128 kN/m
5.3125 pli
Stainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330
Thermal Properties Metric English Comments
CTE, linear 58.0 µm/m-°C
32.2 µin/in-°F
Second heat; ASTM-D696
20.0 µm/m-°C

@Thickness 0.0508 mm
11.1 µin/in-°F

@Thickness 0.00200 in
First heat; ASTM-D696
Electrical Properties Metric English Comments
Dielectric Constant 3.21

@Frequency 1000 Hz
3.21

@Frequency 1000 Hz
0.040 thickness; ASTM D-150-92
Dielectric Strength 13.4 kV/mm

@Thickness 0.0508 mm
340 kV/in

@Thickness 0.00200 in
500 vac, rms. [60 Hz]/sec; ASTM D149-92
Dissipation Factor 0.040

@Thickness 0.0508 mm
0.040

@Thickness 0.00200 in
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Adhesive Type 300