Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.93128 kN/m | 5.3125 pli | to Polypropylene, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330 |
3M 9443NP Double Coated Tapes with Adhesive 700 Series 3M™ Double Coated Tapes with 3M™ Adhesive 700 Series feature a high tack synthetic rubber adhesive which provides excellent quick stick or initial adhesion and bonds together a wide variety of mat.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | to Stainless Steel, 72 hr. dwell, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330 |
3M 9461P Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | to Stainless Steel, 72 hr. dwell, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330 |
3M 9461PC Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | Stainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330 |
3M 9471 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | ABS, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9485PC Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | Stainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330 |
3M 9671 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | Stainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330 |
3M 9673 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | ABS, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9675 Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | Adhesion to PVC; ASTM D1000 |
3M Scotch™ 2234 Cable Jacket Repair Tape 3M™ Scotch™ Cable Jacket Repair Tape 2234 provides a cost effective and efficient means of covering and protecting damaged sections of cable jacket, thereby extending the life of the cable and red.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | Smooth Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7903 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | Smooth Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | Smooth Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | Smooth Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | Smooth Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7908FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | Smooth Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7909 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | Stainless Steel, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330 |
3M 93010LE High Strength Double Coated Tape with Adhesive 300LSE 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | ABS, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330 |
3M 93015LE High Strength Double Coated Tape with Adhesive 300LSE 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | ABS, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9445 Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | Stainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330 |
3M 9471PC Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | ABS, 90° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330 |
3M 9475LEB High Strength Double Coated Tape with Adhesive 300LSE 3M™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryli.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | ABS, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9485EK Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 0.93128 kN/m | 5.3125 pli | to Steel; ASTM D3330 |
3M F-9465PC Adhesive Transfer Tape 3M™ Adhesive Transfer Tape F-9465PC is a 5 mil thick adhesive transfer tape which has been formulated for bonding to many flexible vinyls and to resist the effects of plasticizer migration in flexi.. |