3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7650-S-HSG and 7660-S-HSG Series, are designed for applications requiring a high-ampacity ground. Each kit contains one-piece, skirted, silicone rubber termination with high-ampacity ground assembly and is qualified as IEEE Standard 48 Class 1 for outdoor weather-exposed applications. The termination assemblies consist of a skirted insulator, high-dielectric constant (High-K) stress control tube, conformable High-K stress controlling compound and built-in environmental top sealing compound. The insulator is made of a dark gray silicone rubber with excellent tracking resistance and hydrophobic properties.Information provided by 3M
Mechanical Properties Metric English Comments
Tensile Strength at Break 10.3 MPa
1490 psi
High-K Stress Control Tube; ASTM D412
100% Modulus 0.00110 GPa
0.160 ksi
High-K Stress Control Tube; ASTM D412
300% Modulus 0.00345 GPa
0.500 ksi
High-K Stress Control Tube; ASTM D412
Electrical Properties Metric English Comments
Dielectric Constant 22

@Frequency 60.0 Hz
22

@Frequency 60.0 Hz
High-K Stress Control Tube, 1000 V, 50% RH; ASTM D150
25

@Frequency 60.0 Hz
25

@Frequency 60.0 Hz
High-K Stress Control Compound, 1000 V, 50% RH, 100 mil; ASTM D150
Dielectric Strength 11.8 kV/mm

@Thickness 1.91 mm
300 kV/in

@Thickness 0.0750 in
Environmental Sealing Compound; ASTM D149
Dissipation Factor 0.10

@Frequency 60.0 Hz
0.10

@Frequency 60.0 Hz
High-K Stress Control Tube, 1000 V, 50% RH; ASTM D150
0.90

@Thickness 2.54 mm,
Frequency 60.0 Hz
0.90

@Thickness 0.100 in,
Frequency 60.0 Hz
High-K Stress Control Compound, 1000 V, 50% RH; ASTM D150