Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 10.3 MPa | 1490 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B65U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C75A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 10.3 MPa | 1500 psi | ASTM D638 |
LyondellBasell Petrothene® GA574189 Linear Low Density Polyethylene, Injection Molding Grade PETROTHENE GA574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items.Regulatory Status: GA574189 meets th.. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | ASTM D638 |
Manifattura Cattaneo RULON® LR Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Tensile Strength at Break | 10.3 MPa | 1500 psi | |
Shin-Etsu Silicones SV-13500U Silicone Rubber SV13500U is one of a series of easy processing, general purpose silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendaring. Product F.. |
|||
Tensile Strength at Break | 10.3 MPa | 1500 psi | ASTM D412 |
Teknor Apex Monprene® MP-1883-L2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 10.3 MPa | 1500 psi | ASTM D412 |
Teknor Apex Monprene® MP-2295 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | ASTM D412 |
Sumitomo Chemical ESPOLEX® WT501 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Tensile Strength at Break | 10.3 MPa | 1500 psi | ASTM D412 |
Teknor Apex Telcar® TELC 302 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 10.3 MPa | 1500 psi | ASTM D412 |
Teknor Apex Telcar® TL-1524E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | Type IV specimen, compression molded, crosshead speed 2 in/min; ASTM D638 |
DuPont Nucrel® 599 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Tensile Strength at Break | 10.3 MPa | 1500 psi | ASTM D638 |
ExxonMobil Escorene® LD 713.93 Molding, extrusion and compounding resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer with very good toughness, high clarity and excellent processability. It is suitable for use in making molded articles, extruded profile.. |
|||
Tensile Strength at Break | 10.3 MPa | 1500 psi | ISO 527-2/1A/50 |
ExxonMobil LDPE LD 605BA Low Density Polyethylene Resin (European Grade) Product Description: LD 605BA is a general purpose LDPE grade, characterized by good stiffness and good toughness. It’s easy processable.Availability: Africa & Middle East and Europe Additive: Ant.. |
|||
Tensile Strength at Break | 10.3 MPa | 1500 psi | ASTM D412 |
Compuestos Dominicanos Polycom C-550170 PVC Description: Compuestos Dominicanos, S.A. produces a wide variety of PVC compounds for the injection molding of foot wear products, everything from full injection, shoe soles, boots, and PVC compoun.. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | High-K Stress Control Tube; ASTM D412 |
3M 7620-T Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo.. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | High-K Stress Control Tube; ASTM D412 |
3M 7660-S-HSG Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7650-S-HSG and 7660-S-HSG Series, are designed for applications requiring a high-ampacity ground. Each kit contains one-piece, skirt.. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | High-K Stress Control Tube; ASTM D412 |
3M 7680-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | High-K Stress Control Tube; ASTM D412 |
3M 7690-T Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo.. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | Solvent Resistance |
3M HDT Heat Shrink Tubing 3M Heat Shrink Tubing HDT is a designed to provide reliable performance as well as excellent mechanical and environmental protection. This flame-retardant product combines the important advantage of.. |
|||
Tensile Strength at Break | 10.3 MPa | 1500 psi | ASTM D638 |
ExxonMobil LD 419.MV Wire & Cable Resin
(discontinued **) LD 419.MV is a LDPE designed for wire and cable applications and is suitable for making crosslinkable compounds for medium voltage insulation.Information provided by ExxonMobil Chemical |
|||
Tensile Strength at Break | 10.3 MPa | 1500 psi | ASTM D638 |
Aaron Industries AVPE LD 300-1 MELT 20 Virgin Polyethylene A natural, high flow Low Density Polyethylene resin, specifically designed for high speed injection molding applications. |
|||
Tensile Strength at Break | 10.3 MPa | 1500 psi | ASTM D412 |
Teknor Apex Monprene® MP-2870E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |