Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 10.3 MPa | 1490 psi | |
NEU NeuSoft™ 455-50A Ester/ether TPU / SBC blend |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne FireCon™ CPE 30-2 RoHS BLACK Polyethylene, Chlorinated (CPE) CPE-30-2 RoHS BLACK is a RoHS compliant heavy duty thermoplastic jacket for power and control cables. It is suitable for VW1 and tray fire rated applications. CPE-30-2 RoHS BLACK has a good balance .. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A44565 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B65F1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible D80M0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible FC700 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible P510 Natural Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R246AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | 500 mm/min; ASTM D638 |
Eastman E6837-539A Polyethylene
(discontinued **) PolyethyleneE6837-539A is used in various injection molding applications including closures for containers or extrusion coating for high stiffness. It has good processability. This product may be us.. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2155 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2155 is a 55 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2155 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2155G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2155G is a 55 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2155G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B65U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C7500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C75A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | Type IV specimen, compression molded, crosshead speed 2 in/min; ASTM D638 |
DuPont Nucrel® 599 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | High-K Stress Control Tube; ASTM D412 |
3M 7620-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | High-K Stress Control Tube; ASTM D412 |
3M 7650-S-HSG Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7650-S-HSG and 7660-S-HSG Series, are designed for applications requiring a high-ampacity ground. Each kit contains one-piece, skirt.. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | High-K Stress Control Tube; ASTM D412 |
3M 7680-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | Solvent Resistance |
3M HDT Heat Shrink Tubing 3M Heat Shrink Tubing HDT is a designed to provide reliable performance as well as excellent mechanical and environmental protection. This flame-retardant product combines the important advantage of.. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | High-K Stress Control Tube; ASTM D412 |
3M 7640-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | High-K Stress Control Tube; ASTM D412 |
3M 7690-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
Tensile Strength at Break | 10.3 MPa | 1490 psi | Solvent Resistance |
3M MDT Tubing 3M MDT Tubing offers increased flexibility in combination with excellent abrasion, corrosion and environmental resistance properties and meets MIL-DTL-23053/15, Class 2. Uncoated product (without se.. |