3M™ Vinyl Tape 4712 is a conformable colored (9 colors plus transparent) tapes made from vinyl backing with rubber adhesive. They are ideal for many lane and safety markings, color coding, abrasion protection, masking, sealing, splicing and other general purpose applications. 3M vinyl tape 4712 is a linered version of 3M vinyl tape 471 that may be used for die cutting or large area applications.Information provided by 3M
Physical Properties Metric English Comments
Thickness 63.5 microns
2.50 mil
Liner; ASTM D3652
104 microns
4.10 mil
Backing; ASTM D3652
132 microns
5.20 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 19.3 MPa
2800 psi
ASTM D3574
Elongation at Break 150 %
150 %
ASTM D3759
Peel Strength 0.2849 kN/m
1.625 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 77.0 °C
171 °F
Minimum Service Temperature, Air 4.00 °C
39.2 °F
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Yellow, white, red, black, brown, green, orange, purple, blue and transparent