Polymer Property : Maximum Service Temperature, Air = 77.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 77.0 °C
171 °F
Deflection temperature; load unknown.
Abatron AboCast 8-12/Abocure 8-12 Epoxy  (discontinued **)
2-part solvent-free dielectric epoxy casting compound.Processing: 100/13.2 ratio (pbw); Gel time, 100 g (3.5 oz.): 49 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F..
Maximum Service Temperature, Air 77.0 °C
171 °F
Deflection temperature; load unknown.
Abatron AboCast 8-13/Abocure 8-13 Epoxy  (discontinued **)
2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/12.80 ratio (pbw); Gel time, 100 g (3.5 oz.): 53 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°..
Maximum Service Temperature, Air 77.0 - 87.0 °C
171 - 189 °F
Softening Range
Huntsman Tactix XP 71756.00 Epoxy
Weight per Epoxide (EEW, g/eq) 245 to 265.Comments/Applications: Dicyclopentadiene based epoxy. Functionality 3.2.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquire..
Maximum Service Temperature, Air 77.0 °C
171 °F
Heat Distortion Temp
Hannam Chemical Hanalac 795 ABS, Pipe Grade
Designed for pipe and bobbin sleeves. Excellent processability and high impact strength. Manufactured to prevent static electricity.
Maximum Service Temperature, Air 77.0 °C
171 °F
Heat Distortion Temp
Hannam Chemical Hanalac HFA-700 ABS
Maximum Service Temperature, Air 77.0 °C
171 °F
ChevronTexaco Delo® NLGI 00 Grease EP
FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple..
Maximum Service Temperature, Air 77.0 °C
171 °F
ChevronTexaco Dura-Lith® NLGI 00 Grease EP
FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic..
Maximum Service Temperature, Air 77.0 °C
171 °F
3M 471 Vinyl Tape
3M™ Vinyl Tape 471 is a conformable colored (9 colors plus transparent) tapes made from vinyl backing with rubber adhesive. They are ideal for many lane and safety markings, color coding, abrasion ..
Maximum Service Temperature, Air 77.0 °C
171 °F
3M 4712 Vinyl Tape
3M™ Vinyl Tape 4712 is a conformable colored (9 colors plus transparent) tapes made from vinyl backing with rubber adhesive. They are ideal for many lane and safety markings, color coding, abrasion..
Maximum Service Temperature, Air 77.0 °C
171 °F
3M 5700 Safety Stripe Tape
3M™ Safety Stripe Tapes are durable vinyl tapes used to identify and mark traffic areas and physical hazards.Information provided by 3M
Maximum Service Temperature, Air 77.0 °C
171 °F
3M 5702 Safety Stripe Tape
3M™ Safety Stripe Tapes are durable vinyl tapes used to identify and mark traffic areas and physical hazards.Information provided by 3M
Maximum Service Temperature, Air 77.0 °C
171 °F
Service
3M 7710 Acetate Identification Label Material
3M™ Label Material 7710 gloss clear acetate with 3M™ 400 high tack acrylic adhesive offers consistent, high quality appearance and excellent UV resistance. The transparent film easily die-cuts whi..
Maximum Service Temperature, Air 77.0 °C
171 °F
3M 480 Polyethylene Tape
3M™ Polyethylene Tape 480 has a transparent polyethylene backing with a long aging transparent acrylic adhesive. It can be used for splicing and repairing polyethylene sheeting. It is also recommen..