| CP-Polymer-Technik Wellamid® 6000 CF 18 HWCP 18% Carbon Fiber Nylon 6, Heat Stabilized, Conditioned |
Nylon 6, Carbon Fiber Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 CP Nylon 6, Dry |
Nylon 6, Unreinforced |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 GS 40 HWCP 40% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry |
Nylon 6, Glass Bead Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 GV 10 HWCP 10% Glass Fiber Nylon 6, Heat Stabilized, Dry |
Nylon 6, 10% Glass Fiber Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 GV 20 HWCP 20% Glass Fiber Nylon 6, Heat Stabilized, Conditioned |
Nylon 6, 20% Glass Fiber Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 GV 25 HWUVCP 25% Glass Fiber Nylon 6, UV Stabilized, Heat Stabilized, Conditioned |
Nylon 6, 30% Glass Fiber Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 GV 35 HWCP 35% Glass Fiber Nylon 6, Heat Stabilized, Conditioned |
Nylon 6, 40% Glass Fiber Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 GVS 10/20 HWUVCP 10% Glass Fiber and 20% Glass Sphere Nylon 6, UV Stabilized, Heat Stabilized, Conditioned |
Nylon 6 |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 GVS 10/30 HWCP 10% Glass Fiber and 30% Glass Sphere Nylon 6, Heat Stabilized, Dry |
Nylon 6 |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 GVZ 45 HWCP 45% Glass Fiber Nylon 6, Impact Resistant, Good Surface Finish, Heat Stabilized, Dry |
Nylon 6, 50% Glass Fiber Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 GX 350 HWCP Combination Nylon 6, Heat Stabilized, Conditioned |
Nylon 6 |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 HWCP Nylon 6, Heat Stabilized, Dry |
Nylon 6, Unreinforced |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 MF 30 HWCP 30% Milled Glass Fiber Nylon 6, Heat Stabilized, Conditioned |
Nylon 6, 30% Glass Fiber Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 MR 409 HWCP Mineral Nylon 6, Heat Stabilized, Conditioned |
Nylon 6, 40% Mineral Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 MZ 301 CP Combination Nylon 6, Heat Stabilized, Conditioned |
Nylon 6 |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 SCP Nylon 6, Finely Crystalline, Conditioned |
Nylon 6, Unreinforced |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000/42 GV 15 HWCP 15% Glass Fiber Nylon 6, Polymer Modified, Heat Stabilized, Dry |
Nylon 6, 20% Glass Fiber Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000/50 CP Nylon 6, Impact Modified Until 0°C, Conditioned |
Nylon 6, Impact Grade |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000/52 GV 15 HWUVCP 15% Glass Fiber Nylon 6, Low Temperature Impact Modified, UV Stabilized, Heat Stabilized, Dry |
Nylon 6, Glass Filled, Impact Grade |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000/58 CP Nylon 6, Impact Modified Until -40°C, Conditioned |
Nylon 6, Impact Grade |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000/58 HWUVCP Nylon 6, Impact Modified Until -40°C, UV Stabilized, Heat Stabilized, Conditioned |
Nylon 6, Impact Grade |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 CF10 HWCP 10% Carbon Fiber Nylon 66, Heat Stabilized, Dry |
Nylon 66, 10% Carbon Fiber Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 GS 15 HWCP 15% Glass Sphere Filled Nylon 66, Heat Stabilized, Conditioned |
Nylon 66, Glass Bead Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 GS 30 HWCP 30% Glass Sphere Filled Nylon 66, Heat Stabilized, Conditioned |
Nylon 66, Glass Bead Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 GS 40 HWCP 40% Glass Sphere Filled Nylon 66, Heat Stabilized, Conditioned |
Nylon 66, Glass Bead Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 GV 10 HWCP 10% Glass Fiber Nylon 66, Heat Stabilized, Dry |
Nylon 66, 10% Glass Fiber Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 GV 25 HWCP 25% Glass Fiber Nylon 66, Heat Stabilized, Conditioned |
Nylon 66, 30% Glass Fiber Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 GV 25 HWCP 25% Glass Fiber Nylon 66, Heat Stabilized, Dry |
Nylon 66, 30% Glass Fiber Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 GVS 20/10 HWCP 20% Glass Fiber and 10% Glass Sphere Nylon 66, Heat Stabilized, Dry |
Nylon 66 |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 HW Nylon 66, Heat Stabilized, Dry |
Nylon 66, Unreinforced |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 HWS Nylon 66, Finely Crystalline, Heat Stabilized, Conditioned |
Nylon 66, Unreinforced |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 HWUVCP Nylon 66, UV Stabilized, Heat Stabilized, Conditioned |
Nylon 66, Unreinforced |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 MRGV 20/20 HWCP 20% Mineral and 20% Glass Fiber Nylon 66, Heat Stabilized, Dry |
Nylon 66, Glass/Mineral Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 66, Heat Stabilized, Conditioned |
Nylon 66, Glass/Mineral Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 MZ 401 CP Combination Nylon 66, Conditioned |
Nylon 66 |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 MZ 401 CP Combination Nylon 66, Dry |
Nylon 66 |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 PA-66-HWV0CP UL-Licensed Nylon 66, Flame Protection, Heat Stabilized, Conditioned |
Nylon 66, Unreinforced, Flame Retardant |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600/42 HWCP Nylon 66, Polymer Modified, Heat Stabilized, Conditioned |
Nylon 66, Impact Grade |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600/50 GV 15 HWCP 15% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Dry |
Nylon 66, Glass Reinforced, Impact Grade |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600/506 HWCP Nylon 66, Impact Modified, Heat Stabilized, Conditioned |
Nylon 66, Impact Grade |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600/508 HWUVCP Nylon 66, Impact Modified, UV Stabilized, Heat Stabilized, Conditioned |
Nylon 66, Impact Grade |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600/58 HWCP Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Conditioned |
Nylon 66, Impact Grade |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 GV 25 HWUVCP 25% Glass Fiber Nylon 6, UV Stabilized, Heat Stabilized, Dry |
Nylon 6, 30% Glass Fiber Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 CF 10 HWCP 10% Carbon Fiber Nylon 6, Heat Stabilized, Dry |
Nylon 6, Carbon Fiber Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 GS 25 HWCP 25% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry |
Nylon 6, Glass Bead Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6000 GS 30 HWCP 30% Glass Sphere Filled Nylon 6, Heat Stabilized, Conditioned |
Nylon 6, Glass Bead Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 GS 20 HWCP 20% Glass Sphere Filled Nylon 66, Heat Stabilized, Conditioned |
Nylon 66, Glass Bead Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 GV 10 HWCP 10% Glass Fiber Nylon 66, Heat Stabilized, Conditioned |
Nylon 66, 10% Glass Fiber Filled |
Wellamid®
|
| CP-Polymer-Technik Wellamid® 6600 MR 409 HWCP 40% Mineral Nylon 66, Heat Stabilized, Dry |
Nylon 66, 40% Mineral Filled |
Wellamid®
|