Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.50e+14 ohm-cm | 2.50e+14 ohm-cm | ASTM D257 |
S&E Specialty Polymers GTPO 9100HF Series PVC Application: New generation 80/90C, UV Resistant, low gravity, flexible, polyolefin based Zero Halogen compound with good physical characteristics.Information provided by S&E Specialty Pol.. |
|||
Volume Resistivity | 2.50e+14 ohm-cm | 2.50e+14 ohm-cm | |
Momentive Performance Materials IS808 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, Translucent IS800 series one-component, ready-to-use silicone adhesive sealants have a paste-like consistency and cure to silicone rubber on exposure to atmospheric moisture at room temperature. Because these .. |
|||
Volume Resistivity | 2.50e+14 ohm-cm | 2.50e+14 ohm-cm | |
Momentive Performance Materials IS800.09 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, Aluminum IS800 series one-component, ready-to-use silicone adhesive sealants have a paste-like consistency and cure to silicone rubber on exposure to atmospheric moisture at room temperature. Because these .. |
|||
Volume Resistivity | 2.50e+14 ohm-cm | 2.50e+14 ohm-cm | |
Momentive Performance Materials IS802 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, White IS800 series one-component, ready-to-use silicone adhesive sealants have a paste-like consistency and cure to silicone rubber on exposure to atmospheric moisture at room temperature. Because these .. |
|||
Volume Resistivity | 2.50e+14 ohm-cm | 2.50e+14 ohm-cm | |
Momentive Performance Materials IS803 One-Component, Paste Consistency Silicone Rubber Adhesive Sealant, Black IS800 series one-component, ready-to-use silicone adhesive sealants have a paste-like consistency and cure to silicone rubber on exposure to atmospheric moisture at room temperature. Because these .. |
|||
Volume Resistivity | 2.50e+14 ohm-cm | 2.50e+14 ohm-cm | ASTM D247 |
Plenco 1501 Polyester, Briquette, Transfer Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Volume Resistivity | 2.50e+14 ohm-cm | 2.50e+14 ohm-cm | |
Tra-Con Tra-Bond 240-2 Polyurethane Adhesive TRA-BOND 240-2 polyurethane adhesive is a low outgassing polyurethane adhesive which meets the requirements of NASA specification SP-R-0022. Information provided by Tra-Con Inc. |
|||
Volume Resistivity | 2.50e+14 ohm-cm | 2.50e+14 ohm-cm | |
Tra-Con Tra-Bond 77-2LTC Low Temperature Cure SMD Adhesive TRA-BOND 77-2LTC one component, solvent-free, insulative epoxy adhesive is designed to cure at temperatures as low as 80°C. This adhesive is specifically designed for attaching surface mounted devi.. |
|||
Volume Resistivity | 2.50e+14 ohm-cm @Temperature 23.0 °C |
2.50e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds HL 120 Flexible PVC, Insulation for High Temperatures Operating temperature 110°C |
|||
Volume Resistivity | 2.50e+14 ohm-cm @Temperature 23.0 °C |
2.50e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds AP 95/1 Flexible PVC, Flame Retardant Insulation General purposes |
|||
Volume Resistivity | 2.50e+14 ohm-cm | 2.50e+14 ohm-cm | 50% RH; ASTM D-257 |
Axiall 10805 Wire & Cable Flexible PVC Non-lead stabilized, 75°C rated compound recommended for integral insulation/jacket constructions.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Volume Resistivity | 2.50e+14 ohm-cm | 2.50e+14 ohm-cm | Cured property; ASTM D257 |
Aptek 6505PMF Electronic-grade, non-conductive adhesive APTEK 6506-PMF is a one component, 100% solid, mineral-filled epoxy adhesive specifically designed for the attachment of electronic components to printed circuit boards as well as a protective barri.. |