S&E Specialty Polymers GTPO 9100HF Series PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer S&E Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GTPO 9100HF Series PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: New generation 80/90C, UV Resistant, low gravity, flexible, polyolefin based Zero Halogen compound with good physical characteristics.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
pH 8.42
8.42
IEC 60754-2
Mechanical Properties Metric English Comments
Tensile Strength >= 12.4 MPa
>= 1800 psi
ASTM D638
>= 10.7 MPa

@Treatment Temp. 121 °C,
Time 605000 sec
>= 1550 psi

@Treatment Temp. 250 °F,
Time 168 hour
Air Oven aged
Elongation at Break >= 450 %
>= 450 %
ASTM D638
>= 351 %

@Treatment Temp. 121 °C,
Time 605000 sec
>= 351 %

@Treatment Temp. 250 °F,
Time 168 hour
Air Oven aged
Thermal Properties Metric English Comments
Brittleness Temperature <= -16.0 °C
<= 3.20 °F
ASTM D746
Electrical Properties Metric English Comments
Volume Resistivity 2.50e+14 ohm-cm
2.50e+14 ohm-cm
ASTM D257
Dielectric Constant 2.93

@Frequency 1.00e+6 Hz
2.93

@Frequency 1.00e+6 Hz
ASTM D150-1994
Dissipation Factor 0.0059

@Frequency 1.00e+6 Hz
0.0059

@Frequency 1.00e+6 Hz
ASTM D150-98
Descriptive Properties Value Comments
Conductivity Values 17.92 µS/mm